Skip to content
Depomaterials

Evaporation Materials

Chromium Evaporation Corn (Cr, 4N)

Coarse granular chromium for baffled box sources — a larger charge and fewer chamber openings on long production runs.

A single chromium corn: a solid brushed-metal truncated cone for evaporation sources.
Purity
99.99% (4N)
Lead time
2–4 weeks
Qualified in
Europe
Documentation
Certificate of analysis per batch

Purity up to 99.999%

5N material with certificate of analysis

Quote within 24 h

Technical review by materials engineers

Shipped from Europe

Dispatched inside the EU, customs handled at our end

Custom dimensions

Built to your tool and bonding spec

About chromium evaporation corn

Chromium corn is the same high-purity material as chromium shot in a coarser, irregular granular form. The reason to choose it is charge volume: a box source packed with corn holds substantially more chromium than the same source filled with fine shot, so production runs go longer between chamber openings.

In decorative coating and photomask production, where the same layer is deposited continuously for shifts at a time, the cost of a chamber opening — pump-down time, lost throughput, risk of contamination — dominates the material cost. Corn is the practical answer.

Because chromium sublimes rather than melts, a baffled box source is the usual configuration: the baffle prevents granules being ejected by outgassing and produces a more uniform vapour flux than an open boat.

Chromium Evaporation Corn specifications

Standard specification below. Anything on this table can be changed — send us your drawing or tool model and we will quote to it.

Chromium Evaporation Corn technical specification
Purity99.99% (4N), 99.95% (3N5) standard grade
FormCorn — coarse irregular granules
Granule size3–12 mm typical
Sublimation point~1200 °C
Oxygen content< 200 ppm
Typical sourceBaffled box source, large tungsten boat

Chromium material datasheet

Published constants for chromium — the numbers you need to set up a run before the material arrives. Print this page for the process folder, or send it to us with your parameters and we will tell you whether the grade we stock suits them.

Chemical identity

Chromium Evaporation Corn — chemical identity
MaterialChromium
SymbolCr
CAS number7440-47-3
Atomic number24
Atomic weight51.9961
AppearanceSilvery, metallic

Physical and thermal properties

Chromium Evaporation Corn — physical and thermal properties
Theoretical density7.2 g/cm³
Melting point1,857 °C
Thermal conductivity94 W/m·K
Coefficient of thermal expansion4.9 × 10⁻⁶/K
Z ratio (QCM)0.305

Evaporation process data

Chromium Evaporation Corn — evaporation process data
E-beamGood
Thermal evaporation techniquesBoat: Cr-plated W rods · Coil: W · Basket: W · Crucible: vitreous carbon
E-beam crucible linerFABMATE®, graphite, tungsten
Temperature at 10⁻⁸ Torr837 °C
Temperature at 10⁻⁶ Torr977 °C
Temperature at 10⁻⁴ Torr1,157 °C
Suggested QCM crystalAlloy
Process notesFilms very adherent. High rates possible. Sublimes below its melting point.

Values above are published material constants for process planning and can vary with grade, microstructure and measurement method. They are not a supply specification — what we guarantee on your order is the specification table above and the certificate of analysis shipped with it.

Source: Kurt J. Lesker Company, deposition materials data. CAS numbers from the public chemical registry entry for each element.

Applications

High-volume decorative coating

Chrome-look finishes on consumer hardware, automotive trim and sanitaryware in long production runs.

Photomask blank production

Chromium absorber layers deposited continuously in high-throughput mask blank lines.

Large-area adhesion layers

Cr seed layers under gold on large substrates and panel-level processes.

Optical blocking films

Opaque chromium layers for apertures, encoder scales and reticles.

What we can change for you

  • Granule size graded to match your box source geometry.
  • 4N high purity or 3N5 standard grade depending on application.
  • Bulk quantities with lot traceability for production use.
  • Also available as shot, pellets or plated rod — see our chromium shot page.

Technical notes

Larger charge volume per source fill means fewer chamber openings and more uptime.

Granular form maintains a large, relatively stable emitting surface through the run.

Low oxygen content keeps films dense and the process predictable.

Chromium Evaporation Corn — questions we get asked

When should I choose chromium corn over shot?

Choose corn when run length matters. Its coarser granules pack a larger charge into a box source, so you open the chamber less often. Choose shot for smaller boats and pockets, and where a more uniform, finer packing gives better rate control on thin, thickness-critical layers.

What is a baffled box source and why use it for chromium?

A baffled box source is an enclosed crucible with an internal baffle over the charge. Because chromium sublimes from solid granules, outgassing can eject loose pieces; the baffle contains them and produces a more uniform vapour flux from the exit aperture. It is the standard configuration for production chromium evaporation.

How long does a full charge of chromium corn last?

It depends entirely on source volume, deposition rate and layer thickness. As a rough guide, a well-packed box source running a decorative coating process typically goes several times longer than the same source filled with fine shot. Tell us your source volume and duty cycle and we can size the order.

Is corn the same purity as shot?

Yes — identical material, different granule morphology. We supply both at 4N (99.99%) and 3N5 (99.95%), with the same certificate of analysis and oxygen specification.

Request a quote for chromium evaporation corn

Send your specification and a materials engineer will price it — not a sales form auto-reply. Quotes for chromium evaporation corn are returned within 24 hours.

Drawings, STEP files and photographs can be attached to the form. Prefer to talk it through? Leave a phone number and ask for a call.

What to include

  • Purity grade — 99.99% (4N) is standard
  • Dimensions, tolerances or a drawing
  • Quantity and required delivery date

No drawing? Send photographs of the worn part — we can work from that.